  1. 1. The Corrosive Effect of Chlorine Containing Species on Waterwalls and Superheater Materials in Waste and Biomass-Fired Power Plants

    Author : Erik Larsson; Chalmers tekniska högskola; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; Combustion; Sulfur recirculation; Superheater corrosion; Heavy metal chlorides; Waterwalls; Alkali-induced corrosion; Biomass; Waste;

    Abstract : To increase power generation from waste- and biomass-fired boilers, it is necessary to increase the temperature and pressure of the steam generated. This implies an increase in the temperature both of the waterwalls and of the steam superheaters in the boiler. READ MORE

  2. 2. Superheater corrosion in biomass and waste fired boilers : Characterisation, causes and prevention of chlorine-induced corrosion

    Author : Peter Viklund; Christofer Leygraf; John Nicholls; KTH; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; high temperature corrosion; waste; biomass; superheater tubes; steel; alkali; chlorine; sulphur;

    Abstract : Biomass and waste fired boilers suffer severely from corrosion of critical components such as superheater tubes. In this work high temperature corrosion of superheater alloys, and methods to mitigate the problem, have been investigated by laboratory studies and controlled field exposures in commercial boilers. READ MORE

  3. 3. Deposit Induced Corrosion in Biofuel Combustion

    Author : Petter Andersson; Chalmers tekniska högskola; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; ferritic steel; high temperature corrosion; superheater; waste combustion; CFB; biofuel boiler; waterwall; alkali chloride; deposit induced corrosion; chromate; nickel-based alloy; austenitic steel; martensitic steel; waste boiler;

    Abstract : Deposit induced corrosion is one of the main mechanisms for attack on heat exchangers in biofuel boilers. This severe corrosion decreases the obtainable steam temperature in boilers, thereby the efficiency in production of electricity is reduced. Deposit formation from the gas on superheater tubes are is generally referred to as fouling. READ MORE

  4. 4. Co-firing complex biomass in a CFB boiler : ash transformation, corrosion control and materials selection

    Author : Henrik Hagman; Dan Boström; Rainer Backman; Mats Lundberg; Lars-Erik Åmand; Umeå universitet; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; ash transformation; process control; equilibrium calculations; boiler availability; failures; alloy selection; alloy degradation; vortex finder VF ; service life estimation; sulfation; chloridation; high temperature corrosion; biomass; waste derived fuels; forest residues; RDF; Biomal; slaughterhouse waste; peat; waste wood; industrial waste water treatment sludge; HAD; RSMT; Alloy 253MA; Alloy 310S; Alloy 800H HT; Alloy DS; Alloy 600;

    Abstract : The effects of greenhouse gas net emissions on global warming, stricter legislation on waste handling, and the pursuit of ever cheaper heat- and power production are all important factors driving the introduction of complex fuels in incineration plants. However - without fundamental knowledge regarding ash transformation, corrosion control, and materials selection – this introduction of potentially economically and environmentally beneficial fuels, might instead cause economic loss and environmentally adverse effects. READ MORE

  5. 5. High temperature corrosion during waste incineration : characterisation, causes and prevention of chlorine-induced corrosion

    Author : Peter Viklund; Christofer Leygraf; Jan Froitzheim; Staffan Hertzman; Sweden Stockholm Swerea KIMAB AB; []
    Keywords : NATURVETENSKAP; NATURAL SCIENCES; high temperature corrosion; waste incineration; superheater tubing; steel; alkali; chlorine; suphur; Chemistry; Kemi;

    Abstract : Waste-fired boilers suffer severely from corrosion of critical components such as superheater tubes. In this work the high temperature corrosion of candidate superheater alloys have been investigated by detailed laboratory studies and controlled field exposures in full-scale boilers. READ MORE