Search for dissertations about: "corrosion welding"
Showing result 1 - 5 of 31 swedish dissertations containing the words corrosion welding.
-
1. The Role of Microstructure in the Atmospheric Corrosion of Selected Light Alloys and Composites
Abstract : Magnesium-aluminum (Mg-Al) alloys, Mg-based metal matrix composites (MMCs) and Al alloys are among the best material candidates for future lightweight solutions. However, the use of these materials is limited by a number of issues, including the ability to resist corrosion. READ MORE
-
2. Use of localised techniques to elucidate the influence of process variables on the corrosion of stainless steels
Abstract : Several factors during steel manufacture and fabrication can alter the passivity and corrosion behaviour of stainless steels. These include alloying, deformation, welding and heat treatments. READ MORE
-
3. High Temperature Corrosion of FeCrAl Alloys in Biomass- and Waste-fired Boilers - The Influence of Alloying Elements in Prediction and Mitigation of Corrosion in Harsh Environments
Abstract : Combustion of biomass and waste for heat and power production is an alternative to fossil fuels and can be an important step towards a more sustainable future. The electrical efficiency of the fuel-to-energy conversion process is largely dependent on the steam parameters (temperature and pressure) of the combined heat and power (CHP) plants. READ MORE
-
4. Friction stir welding of copper canisters for nuclear waste
Abstract : The Swedish model for final disposal of nuclear fuel waste is based on copper canisters as a corrosion barrier with an inner pressure holding insert of cast iron. One of the methods to seal the copper canister is to use the Friction Stir Welding (FSW), a method invented by The Welding Institute (TWI). READ MORE
-
5. Use of local electrochemical techniques for corrosion studies of stainless steels
Abstract : The excellent corrosion resistance of stainless steels arises from the presence of a passive film on its surface. Above 10.5wt% Cr a chromium oxide of 1-3 nm is formed on the surface of the metal that in case of damage will reform and hinder further dissolution of the metal. READ MORE