  1. 1. Corrosion and Surface Studies of Stainless Steel and Chromium Carbide Thin-Films

    Author : Jonas Högström; Leif Nyholm; Kristina Edström; Patrik Schmutz; Uppsala universitet; []
    Keywords : NATURVETENSKAP; NATURAL SCIENCES; corrosion; electrochemistry; thin film; stainless steel; passive film; chromium carbide; carbon oxidation; surface; depth profile; XPS; SEM; EQCM; sputtering;

    Abstract : Although the passive films that form on stainless steels have been extensively studied, the concentration depth profiles are not fully understood. Their thinness makes passive films hard to study, but angle-resolved X-ray photoelectron spectroscopy (ARXPS) is a non-destructive technique that can be used to obtain depth information. READ MORE

  2. 2. Hydrogen embrittlement and corrosion behavior of low-temperature carburized austenitic stainless steel

    Author : Xiao Qin; Chalmers tekniska högskola; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; low-temperature carburising; hydrogen embrittlement; Austenitic stainless steel; microstructure; corrosion behavior; expanded austenite;

    Abstract : For metallic components used in hydrogen environments, hydrogen embrittlement and corrosion have always been important considering potential failure risks. Among many metallic materials, austenitic stainless steel has found broad application because of its excellent corrosion and hydrogen embrittlement resistance. READ MORE

  3. 3. Corrosion of steel in concrete at various moisture and chloride levels

    Author : Johan Ahlström; Avdelningen för Byggnadsmaterial; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; steel; rebar; concrete; corrosion; chloride threshold level; moisture;

    Abstract : About 7000 concrete bridges in Sweden were built before 1965. The annual cost for maintenance of these bridges is about 0.6% of their total value. The cooling water tunnels at Swedish nuclear power plants have been exposed to seawater for about 30-40 years. READ MORE

  4. 4. High Temperature Corrosion Behavior in Biomass- and Waste-Fired Boilers - Insights into catastrophic corrosion and corrosion mitigation techniques

    Author : Julien Phother Simon; Chalmers tekniska högskola; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; 3D tomography; TEM; Sulfur Recirculation; Waste; High-temperature corrosion; Biomass; Coatings; Stainless steel; Ni-based alloys; Deposits; KCl-induced corrosion;

    Abstract : Carbon dioxide is contributing to the greenhouse effect and a significant part comes from the use of fossil fuels. Utilizing more renewable fuels is therefore a solution to decrease the net release of CO2 emissions to the atmosphere. READ MORE

  5. 5. Superheater corrosion in biomass and waste fired boilers : Characterisation, causes and prevention of chlorine-induced corrosion

    Author : Peter Viklund; Christofer Leygraf; John Nicholls; KTH; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; high temperature corrosion; waste; biomass; superheater tubes; steel; alkali; chlorine; sulphur;

    Abstract : Biomass and waste fired boilers suffer severely from corrosion of critical components such as superheater tubes. In this work high temperature corrosion of superheater alloys, and methods to mitigate the problem, have been investigated by laboratory studies and controlled field exposures in commercial boilers. READ MORE