  1. 1. Nickel-Based Single-Crystal Superalloys : the crystal orientation influence on high temperature properties

    Author : Mikael Segersäll; Johan Moverare; Kjell Simonsson; Daniel Leidermark; Roger Reed; Linköpings universitet; []
    Keywords : ;

    Abstract : Superalloys are a group of materials that are used in high temperature applications, for example gas turbines and aero engines. Gas turbines are most commonly used for power generation, and it is only the very critical components which are exposed to the most severe conditions within the turbine, which are made from superalloy material. READ MORE

  2. 2. Characterisation of Nickel-Based Superalloys Manufactued by Electron Beam Melting

    Author : Annika Strondl; Chalmers University of Technology; []
    Keywords : TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEM; electron beam melting; APFIM; EBSD; XRD; DTA; nickel-based superalloys; SEM; additive manufacturing; EDS;

    Abstract : Nickel-based superalloys have been manufactured by electron beam melting (EBM). EBM is an additive manufacturing process for direct production of metal parts. The part is build up by successive melting of metal powder layers in a vacuum chamber using electron beam. READ MORE

  3. 3. Hot Cracking and Grain Boundary Weaknesses of Nickel - Based Superalloys

    Author : Joel Håkan Andersson; Chalmers University of Technology; []
    Keywords : Hot cracks; Notch rupture testing; Eutectic; Weldability; Varestraint testing; Grain boundary weaknesses; Superalloys;

    Abstract : Abstract Grain boundary weaknesses of nickel-based superalloys not only materialize during service in the hot turbine engine sections but also during the weld manufacturing. The performance, in this respect, of the most commonly used alloys at Volvo Aero Corporation (VAC), 718 and the higher temperature capacity Waspaloy, are therefore the main subjects for this thesis. READ MORE

  4. 4. Alloy Design and Characterization of γ′ Strengthened Nickel-based Superalloys for Additive Manufacturing

    Author : Jinghao Xu; Johan Moverare; Ru Lin Peng; Eric Jägle; Linköpings universitet; []
    Keywords : ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; Nickel-based superalloy; Alloy design; Laser powder bed fusion; Cracking susceptibility; Additive manufacturability; Heat treatment; γ′ precipitate; High-temperature mechanical property; Creep.;

    Abstract : Nickel-based superalloys, an alloy system bases on nickel as the matrix element with the addition of up to 10 more alloying elements including chromium, aluminum, cobalt, tungsten, molybdenum, titanium, and so on. Through the development and improvement of nickel-based superalloys in the past century, they are well proved to show excellent performance at the elevated service temperature. READ MORE

  5. 5. Surface Integrity and Fatigue Performance of Nickel-based Superalloys

    Author : Zhe Chen; Ru Peng; Johan Moverare; Sten Johansson; Manuel François; Linköpings universitet; []
    Keywords : ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; TEKNIK OCH TEKNOLOGIER; TEKNIK OCH TEKNOLOGIER; TEKNIK OCH TEKNOLOGIER; ENGINEERING AND TECHNOLOGY; ENGINEERING AND TECHNOLOGY;

    Abstract : Due to global warming, the demand for more efficient gas turbines has increased. A way to achieve this, is by increasing the operating temperature of the gas turbine. Therefore, nickel-based superalloys have been developed to withstand these extreme temperatures and loads, especially in the hot sections. READ MORE