Search for dissertations about: "nickel-based superalloys"
Showing result 11 - 15 of 31 swedish dissertations containing the words nickel-based superalloys.
-
11. Aluminide Diffusion Coatings for Ni Based Superalloys. Coating and Oxide Microstructure
Abstract : This thesis reports on investigations of high temperature oxidation resistant aluminide diffusion coatings for Ni based superalloys. Such coatings basically consist of a .BETA.-NiAl layer at the surface of the . READ MORE
-
12. Microstructure of Pt modified aluminide diffusion coatings on Ni based single crystal superalloys
Abstract : .... READ MORE
-
13. Weld Cracking of Precipitation Hardening Ni-based Superalloys - Investigation of repair welding characteristics and susceptibility towards strain age cracking
Abstract : High temperature resistance and strength requirements make nickel-based superalloys the material of choice for the hot section of aero engines. Fabrication in terms of combining wrought and cast parts in the manufacturing of hot structural components enables component optimisation via the use of wrought high-strength parts, where geometrical constraints allow, and cast parts to produce complex geometries. READ MORE
-
14. Weldability of Cast Superalloys - Effect of homogenization heat treatments on hot cracking susceptibility of cast Alloy 718, ATI® 718Plus®, and Haynes® 282®
Abstract : Precipitation hardened Ni- and Ni–Fe-based superalloys are used in high-temperature sections of aero engines owing to their superior mechanical properties compared to those of the other alloys. However, their better mechanical performance is accompanied by its own challenges during the manufacturing process. READ MORE
-
15. Creep modeling and first-principles investigation of high-temperature alloys
Abstract : Stainless steels and nickel-based superalloys are materials that have been widely used to manufacture components servicing at high temperatures. Creep strength is one of the most important properties in such conditions. READ MORE